What difference would there be in the density of shotcrete before and after shooting? Is there any shotcrete mixture-design software in SI units available? Or any document of shotcrete mixture design in SI units for optimizing shotcrete design?

Shotcrete is simply a placing method for concrete. Thus, the mixture design and material properties are the same as concrete. We are not aware of any software specific to shotcrete in any units. ACI 506R-05, “Guide to Shotcrete”, has guidance on desirable mixture characteristics (aggregate grading, supplemental cementitious material [SCM], and so on) that would be helpful in developing a concrete mixture design for shotcrete placement.

Is there is a manufactured depth gauge that would be glued/nailed to the form to allow the nozzleman to physically see how much concrete is being applied to the surface? We have a condition where there will be two or three applications on the same surface, and I am concerned that the correct depth is not being applied in each pass.

ACI 506R-05, “Guide to Shotcrete,” Section 5.6, on Alignment Control (refer to ASA Bookstore: https://shotcrete.org/bookstore/ProductDetail.aspx?itemid=506R-05) gives specific guidance on proven methods to establish the line and grade of the surface, as well as proper material thickness and cover. Common methods are use of ground wires, guide strips, depth gauges, and depth probes. Please refer to “ASA’s Buyers Guide” (https://shotcrete.org/products-services-information/buyers-guide/) and contact one of our members who provides supplies to the shotcrete industry

Is there a specification with regard to cold joints when using shotcrete?

Generally, the interface between sequentially placed layers of shotcrete is not considered a cold joint because the shotcrete abrasion, velocity of impact, and high paste content make excellent bonding conditions. Cores taken through layers of shotcrete on shotcrete often show that it is virtually impossible to ascertain one layer of shotcrete from the next. Please refer to ACI 506R, “Guide to Shotcrete,” for information on joints in shotcrete.

I would like to know the standard operating procedures for cleaning out shotcrete hoses with air and/or water and, in particular, how to keep the hose from whipping when using air.

Shotcrete hoses can be cleaned out using either water or air. In many instances, the site conditions make cleaning with water not feasible. When cleaning with air, the free end or discharge end of the hose should be secured to something to ensure that the hose does not whip as the material and cleaning ball or rag discharges.

I would appreciate if you could comment on a city of Los Angeles shotcrete code that requires that shotcrete lifts not exceed 3 ft (1 m) and that 3 hours must pass before the second lift can be applied. First of all, if you waited 3 hours between lifts, you would have full-length cold joints along the whole length of the wall. You’d also have to wash out the pump after every lift or the concrete would harden in the pump and hoses. Second, you can’t leave a 4000 to 5000 psi (28 to 34 MPa) mixture sitting in the truck for 3 hours! Does it make any sense to you?

This provision has been an issue for shotcrete contractors in the region for many years. ASA and ACI Committee 506, Shotcrete, do not endorse the concept stated in the “Los Angeles Bulletin.” Unfortunately, this provision has shown up in other areas around the country.
A good shotcrete practice is to limit lift height to that which can be placed without sloughing or sagging and to place subsequent lifts at such a time that the previous lift is sufficiently firm to support the subsequent lift. ACI 506R-05, “Guide to Shotcrete,” Section 8.5.8, specifically addresses this point. The following is a link to ASA’s bookstore:  https://shotcrete.org/bookstore

When was the 4000 psi (28 MPa) standard set for shotcrete?

ASA has taken the position that structural shotcrete is shotcrete that meets or exceeds a compressive strength of 4000 psi (28 MPa). Looking at pertinent ACI Codes related to watertight concrete, as we would expect in a pool, we find ACI 318-95, “Building Code Requirements for Structural Concrete,” introduced a provision in 1995 that required: “Concrete intended to have low permeability when exposed to water shall have a Minimum f´c of 4000 psi (28 MPa)”. Similarly, ACI 350-01, “Code Requirements for Environmental Concrete Structures,” first issued in 2001 required: “Concrete intended to have low permeability when exposed to water, wastewater, and corrosive gases shall have a Minimum f´c of 4000 psi (28 MPa)”. Since ACI 350 is more directly applicable to water-containing structures, the 2001 date is probably the most relevant, though ACI 318 introduced the concept in 1991. We do, however, see shotcrete specified at lesser levels for different types of uses.

What is the standard method for steel fiber-reinforced shotcrete (SFRS) testing? Are you supposed to core test panels or do you only do that for plain shotcrete? Additionally, is round panel toughness testing on SFRS standard today in the United States?

SFRS is routinely cored from shotcrete test panels or in-place shotcrete linings without difficulty. The shotcrete should, however, have a minimum compressive strength of about 10 MPa (1450 psi) at the time of coring.
Round panel testing of flexural toughness of fiber-reinforced shotcrete to ASTM C1550 is often specified and used for quality control (QC) purposes in tunneling and mining projects in North America and elsewhere (for example, mines in Australia) virtually every day of the year.

By subscribing here, you gain access to ASA’s informative monthly e-Newsletter, ‘What’s in the Mix,’ and receive notifications for the current digital format of Shotcrete magazine.

‘What’s in the Mix’ – will keep you updated on ASA’s latest issues of Shotcrete magazine, services, events, and other initiatives.

Shotcrete magazine – an email notification will be sent when a new issue is available online. Please note that hard copies of the magazine are exclusively offered as a member benefit. If you wish to receive a hard copy, kindly visit Join ASA.

To ensure the delivery of emails, make sure you add [email protected] to your “allowed e-mail addresses.”

ASA e-Newsletter — Subscribe

We will be blasting close to a shotcrete wall. Can you suggest any precautionary measures or offer lessons learned when blasting next to a recently shotcrete wall?

It is very common in drill and blast operations to blast shortly after the application of shotcrete. There are certainly risks involved, but a knowledgeable and experienced mining crew working with or for a knowledgeable, experienced contractor would not have any problem with this type of application.

A knowledgeable contractor will develop a mixture and procedures to ensure that the timing of the subsequent blast is compatible with the set time of the shotcrete. Preconstruction testing should be required to establish the set time (both early and final set) to assist in developing the sequence of operations. The set time will also be impacted by the site conditions, such as temperature.